The wind turbine rotor is alloy steel 42CrMo and Q235B dissimilar steel structure
the SMAW and MAG hybrid welding are used to perform the welding experiments. Through metallographic microscope
universal mechanical testing machine and scanning electron microscope analysis
the microstructure properties and appearance of fracture of the welded joints are observed and analyzed.The results show that the increase of welding heat input will reduce the bending properties and low temperature impact properties of welded joints of 42CrMo and Q235B
in the actual welding of motor
the welding heat input
preheat temperature and interpass temperature should be controlled;the microstructure
mechanical properties and the appearance of impact fracture and other technical indicators of welded joints in the 42CrMo and Q235B dissimilar steels prepared by a welding technology with a small heat input all meet the relevant standards
which provides strong technical support for the welding of motor rotor.